I did some work in the past (4-5 years ago) with n-propyl bromide cleaners
and found that they did leave undesirable amounts of surface bromide on the
surface of cleaned assemblies. The free bromine was of a level I usually
equated with electrochemical failures. The solvents may have improved
since that time, but it is something to watch out for.
Doug Pauls
Rockwell Collins.
---------------------------------------------------