Hi folks! Bev is correct - using a vacuum can actually impede moisture
removal if the process is not correctly controlled. I have seen a very neat
demonstration where a container of water is subjected to a relatively fast
vacuum cycle and you can observed the water surface convert to thick layer
of ice! There are a number of investigations which shown that baking is a
more efficient method of moisture removal but the downside is the
degradation of the solderable surface finishes (which does not happen in
the vacuum process).
Dave Hillman
Rockwell Collins
[log in to unmask]
Bev Christian
<[log in to unmask] To: [log in to unmask]
ET> cc:
Sent by: TechNet Subject: Re: [TN] Baking IC's to J-STD-033 that are not in a suitable packaging
<[log in to unmask]>
02/17/2004 09:37
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to Bev
Christian
Reuven,
I have always wondered about that! Faster? And what about part
reliability? In the cases where the elimination of water is not diffusion
controlled, yes, it would be faster. However, if diffusion is the limiting
step for the water coming to the surface of the component, then it does not
make any difference how fast you draw it off the surface. In fact, I
wonder if you could evaporate it fast enough (at lower temperatures and
high vacuum) that you could freeze the water, thus making the water act as
its own plug and limiting you to the sublimation of the surface ice? And
what about dropping the external pressure and thus decreasing the boiling
point of the water so it flash evaporates even easier? Couldn't this then
cause popcorning at, say 60C? I don't know, I'm asking.
regards,
Bev Christian
Research in Motion
-----Original Message-----
From: Reuven ROKAH [mailto:[log in to unmask]]
Sent: February 17, 2004 9:42 AM
To: [log in to unmask]
Subject: Re: [TN] Baking IC's to J-STD-033 that are not in a suitable
packaging
I recommend to be more careful with BGAs components (drying before
production).
Vacuum oven is recommended for low temp. packages. (faster).
Best Regards
ROKAH Reuven
Kathy Kuhlow
<[log in to unmask] To: [log in to unmask]
OM> cc:
Sent by: TechNet Subject: Re: [TN] Baking
IC's to J-STD-033 that are not in a suitable packaging
<[log in to unmask]
>
17/02/2004 16:24
Please respond
to "TechNet
E-Mail Forum.";
Please respond
to Kathy Kuhlow
We have a sealer, MBB bags, Labels, Desiccant, and indicator cards. When
we kit to a work order we open the package count out what is needed. Then
we repack both packages with the necessary items. The parts are put to the
kit and the inventory is returned. When any bag is cut open we look at the
indicator card and if the card is pink we bake them then. That way we
don't have production waits for the rebaking process. If production
returns moisture exposed parts we rebake prior to reinventory. Per 033 we
look at this as described under 8.2.
Kat
>>> [log in to unmask] 02/17/04 03:25AM >>>
Hi,
What is the general working practice when say a class-3 device comes
in vacuum shrinked wrapped with desicant and humidity indicator card
but is in tubes/sticks packaging or even sometimes in reels.
If the whole reel or pack of tubes are not all used up before the floor
life
expires and in theory the devices need to be re-processed @ 125 deg-C
for 24-hours??
I am wondering what most companies do regarding oven processing??
Any knowledge of this would be interesting.
Thanks,
> Douglas I McCall
> Printed Circuit Board Assembly Engineer,
>
> /// /// /// BOC EDWARDS
H BOC Edwards, 15 Marshall Road, Eastbourne, East Sussex, England, BN22
9BA
> * +44 (0)1323 501147
* +44(0)1323 509824
*+44 (0)7785 247 685
> * mailto:[log in to unmask]
>
>
***********************************************************************
This email is confidential and intended solely for the use of the
individual to whom it is addressed. Any views or opinions presented are
solely those of the author and do not necessarily represent those of the
BOC Group plc or any of its affiliates. If you are not the intended
recipient, be advised that you have received this email in error and that
any use, dissemination, forwarding, printing, or copying of this email is
strictly prohibited. If you have received this email in error please return
the message to the sender by replying to it and then delete the message
from your computer.
This footnote also confirms that this email message has been checked by
anti-virus software for the presence of computer viruses. However, the BOC
Group plc or any of its affiliates accepts no responsibility for any virus
or defect that might arise from opening this e-mail or attachments.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|