20% of our assemblies are Immersion silver, All fine pitch SMT boards (25
mil or less) are speced as I.S. We have been transitioning away from HASL
for 2 years now. Any respins get I.S. called out in anticipation of Lead
Free requirements.
Dave C.
-----Original Message-----
From: Franklin D Asbell [mailto:[log in to unmask]]
Sent: Tuesday, February 17, 2004 11:30 AM
To: [log in to unmask]
Subject: [TN] Another view of lead-free
I'm curious where are this "lead-free" activity is occuring?
Looking at our orders over the past 5 years or so I do not see a significant
decline in orders for HASL...containing 40% lead... we've installed
immersion tin, working on immersion gold, have already got electrolytic
gold, we have immersion silver, Entek, etc etc but we still receive a steady
stream of orders for the good 'ol 60/40 coating...should I expect some
trickle-down soon?
I'm just curious is all...
Franklin
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|