Too much flux, or more precisely flux remaining on the mask for too long may
also affect (degreade) the mask and could cause flaking.
Where are you seeing this at? over ground planes? on traces? glass? are you
seeing it before processing? (bare boards) are they using LPI or UV mask?
what color? do you observe contamination os discoloration in the area after
the mask has flaked off?
Franklin
----- Original Message -----
From: "Suzanne Foulkes" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, February 09, 2004 11:09 AM
Subject: [TN] Solder Mask Flaking
I know this was up for a discussion a few weeks ago. Can anyone tell me
what the root cause was determined to be?
I am experiencing solder mask flaking on a group of boards manufactured
by one certain supplier. It is a random occurrence for example 10 out of
the 100 boards we had this occurr. Then a different board we ran 8 out
of 40 were flaking same supplier as previous one.
Supplier runs samples at his facility and he see's no flaking. We
changed our solder temperature from 500 degrees to 450 degrees at the
suppliers suggestion and flaking still occurs. He then states maybe were
not using enough flux but review shows plenty of flux if anything maybe
were using to much flux from the way the boards look coming out of the
wave and washer.
Thanks
Sue Foulkes
QA Manager
AESCO Mfg.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|