In my previous job (big telecom OEM), I personnaly used this geometry and it
worked fine with us:
Pad Length of 0.050", Pad Width of 0.056" & Overall of 0.130".
In my new job now, we use Pad Length of 0.055", Pad Width of 0.055" &
Overall of 0.145". This also prooved to be a winning geometry.
Eric
-----Original Message-----
From: Mike McMonagle [mailto:[log in to unmask]]
Sent: Wednesday, February 04, 2004 3:30 PM
To: [log in to unmask]
Subject: [TN] 0805 Pad Geometry
Looking for feedback on what pad geometries are being used these days
for standard 0805 chips. We are primarily a high-rel, low volume high
temp alloy shop, but have recently pulled in a standard Sn63 board in
volume that the customer is looking for a little layout assistance on.
Pad dimensions are way too large and pad-to-pad spacing too tight,
contributing to big fillets and squeeze balls at the component edges. It
could be worked through aperture changes in the stencil, but the fab is
being spun for another reason anyway so now's a good time to fix 'em up.
Seems that almost every component manufacturer is calling out there own
pad preferences, many of which are contradictory to IPC design
guidelines. Also, any new comments on the pros and cons of using pads
that are slimmer than the termination width of the component? TIA for
the insights....
Mike
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|