You should take care to the cleanliness of the PCBs after the process.
If the PCBs have plugging via holes, active residues can be left there and
it almost impossible to remove them.
Also solder balls from the HASL process can be created in via holes.
The good things are that the PCBs have new finish (solderability) and 100%
thermal stress.
Best Regards
ROKAH
Eddie Rocha
<[log in to unmask] To: [log in to unmask]
om> cc:
Sent by: TechNet Subject: Re: [TN] Rework Gold Finish
<[log in to unmask]
>
04/02/2004 19:48
Please respond
to EddieR
If the amount of gold is less than ~20 uin, then rework might be an
option. Too much gold will result in embrittlement issues with your
solder joints.
On 4 Feb 2004 at 8:47, Ezequiel Cruz wrote:
Can anyone help with the following:
My board house built my boards with a gold finish.
The finish should have been selective gold as we have some
contact areas on
the pwb.
I have insisted on a re-build which is currently being done. However,
because of our all ready late schedule, the board house has offered
to re-
work the gold finish boards for us. The method explained to me was
mask the
selective gold areas and flux clean the remaining board while
dipping in
molten solder.
Does anyone have any experience with re-working this way. Our
biggest
concern is from a re-liability standpoint. Obviously this board will go
through additional thermal cycling not necessarily part of a standard
build. What effect, if any, will this have on the board itself.
Remember
that our stuffing house will place this board through additional
thermal
cycling.
Any help is greatly appreciated.
Ezequiel Cruz
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV
1.8e
To unsubscribe, send a message to [log in to unmask] with
following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-
509-9700 ext.5315
-----------------------------------------------------
-- Thanks,
Eddie Rocha
(408) 978-8992 x 282
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|