That's what I was thinking. Could that be why Poh's rubber squeegee worked, because it was scavenging some of the solder out of the apertures?
Gary Camac
"Allen T. Maddox" wrote:
> Sounds a little like too much solder volume. Maybe a good idea to reduce the aperture.
>
>
> Allen Maddox
> Sr. PC Board Designer
> GAI-Tronics, Corp
> 610-796-5854
> PO Box 1060
> Reading, PA 19607-1060
>
> [log in to unmask]
> www.gai-tronics.com
>
> >>> [log in to unmask] 02/17/04 06:56PM >>>
> We have a new assy. that uses 1206 capacitor networks. We are have a serious
> problem with bridging and unsoldered connections. We think we may have solved
> the non soldered problem by increasing the soak before reflow but still have
> the bridging. Anybody have similar experiences? We are using a 5 mil.
> stencil. The other parts all seem to solder well. We are considering having
> the apertures for these parts reduced. Any suggestions would be greatly
> appreciated.
>
> Charles Caswell
> The Big Kahuna
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
> **********************************************************************
> This email and any files transmitted with it are confidential and
> intended solely for the use of the individual or entity to whom they
> are addressed. If you have received this email in error please notify
> the system manager.
>
> This footnote also confirms that this email message has been swept
> for the presence of computer viruses.
>
> www.hubbell.com - Hubbell Incorporated
> **********************************************************************
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|