Ramon,
I have dealt with the Vigon A200. It is a good product. However we recently
switched to the Kyzen Aquanox 4512P. The difference between these two is
that teh Vigon requires a high concentration of chemical (Around 20%) while
the Kyzen requires only 4%. We had no problems with the Vigon except the
cost.
Dan D.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Dehoyos, Ramon
Sent: Tuesday, February 17, 2004 2:33 PM
To: [log in to unmask]
Subject: [TN] Cleaning Chemistry
Hi Yo'all:
One of our board vendors has changed their cleaning agent to
Vigon A 200 for their in line cleaning. Their in line cleaner is an
Electrovert Aquastorm. Does anybody have any experience with this agent?
Vigon A 200 is suppossed to be good for medium to high pressure.
TIA.
Ramon
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|