TECHNET Archives

February 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "McCall,Doug" <[log in to unmask]>
Date:
Tue, 17 Feb 2004 08:25:45 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Bev Christian <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Bev Christian <[log in to unmask]>
Parts/Attachments:
text/plain (66 lines)
Doug,
Unfortunately ALL our components come in reels and we cannot heat at 125C - there are nasty consequences, trust me.  Look in J-STD-033 for other heating regimes.
Bev Christian
research in Motion

-----Original Message-----
From: McCall,Doug [mailto:[log in to unmask]]
Sent: February 17, 2004 4:25 AM
To: [log in to unmask]
Subject: [TN] Baking IC's to J-STD-033 that are not in a suitable
packaging


Hi,

What is the general working practice when say a class-3 device comes
in vacuum shrinked wrapped with desicant and humidity indicator card
but is in tubes/sticks packaging or even sometimes in reels.

If the whole reel or pack of tubes are not all used up before the floor life
expires and in theory the devices need to be re-processed @ 125 deg-C
for 24-hours??

I am wondering what most companies do regarding oven processing??

Any knowledge of this would be interesting.

Thanks,
> Douglas I McCall
> Printed Circuit Board Assembly Engineer,
>
> /// /// ///  BOC EDWARDS
H   BOC Edwards, 15 Marshall Road, Eastbourne, East Sussex, England, BN22
9BA
> *  +44 (0)1323 501147
*    +44(0)1323 509824
*+44 (0)7785 247 685
> *  mailto:[log in to unmask]
>
>

***********************************************************************
This email is confidential and intended solely for the use of the individual to whom it is addressed. Any views or opinions presented are solely those of the author and do not necessarily represent those of the BOC Group plc or any of its affiliates. If you are not the intended recipient, be advised that you have received this email in error and that any use, dissemination, forwarding, printing, or copying of this email is strictly prohibited. If you have received this email in error please return the message to the sender by replying to it and then delete the message from your computer.

This footnote also confirms that this email message has been checked by anti-virus software for the presence of computer viruses. However, the BOC Group plc or any of its affiliates accepts no responsibility for any virus or defect that might arise from opening this e-mail or attachments.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2