Hello Tom,
With rosin fluxes, you may find a simple black light will illuminate
residues. Alternatively, you can create a stronger illumination via mixing
in fluorescence with your flux. We have some at AAT if you want to give it
a try.
Shean Dalton
Austin American Technologies
Ph: (+1) 512-335-6400 ext. 20
12201 Technology Blvd
Austin, Texas 78727
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Tom Gervascio
Sent: Monday, February 16, 2004 8:00 AM
To: [log in to unmask]
Subject: [TN] fluorescing agents
Does anyone know of a liquid fluorescing agent that I can blend in with some
no -clean rosin fluxes and solder pastes? I'm trying to do some qualitative
cleaning tests under low standoff SMT components.
Thanks
Tom Gervascio
Senior Process Engineer
Sparton Electronics
(352) 540-4040
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|