Steve,
I saw this once many years ago with a UV cured LPI mask. The UV lamp was
not working and the SM got only a thermal dry with no real cure.
John Maxwell
At 04:01 PM 1/13/2004 -0500, you wrote:
>Hi All!
>
>You're probably wondering; "What the heck? Snake board?" That's what I call
>it.
>
>Built this assembly (all PTH), waved it, and then washed it, went to get it
>out of our cleaner, and all the solder mask is coming off in big slabs just
>like a snake does when he sheds his skin! Go look at "Mask Peel, Mask Peel
>2, &
>Mask Peel 3" at:
>
>http://www.stevezeva.homestead.com
>
>I wash in a Electrovert MCS-1000 with Kyzen XJN, and the mask on the board
>was a Dupont Vacrel dry film. Never have had a problem with Vacrel dry films.
>
>The mask doesn't look degraded, or damaged in any way...it's just not stuck
>to the board! Anybody ever seen this happen before? Unfortunately, this was a
>rather expensive assembly.....:^{
>
>Nice way to start the year off, huh?
>
>-Steve Gregory-
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|