Hi All!
Back on January 6, Wee Mei had asked me to post some pictures for him, and
then he posted the question below.
Well, I've been gone since the beginning of the week (up in nice, warm,
Burlington, Ontario Canada), and am just now getting around to posting his pictures
for him. You can see the pictures at: http://www.stevezeva.homestead.com
and look at "soldermask 1-3"
-Steve Gregory-
> ----- Original Message -----
> From: "Lum Wee Mei" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Tuesday, January 06, 2004 1:45 AM
> Subject: [TN] Solder Mask Defects - What casue it.
>
>
> > Hello,
> >
> > I have asked Steve to download the picture at his site. Once it ready,
> > can someone take a look and give me your opinion what is the likely cause.
> >
> > Background : The board was partially mounted previously. It come back
> > to mount the remaining 6 chips. The board was washed as per normal with
> > Ensolv and assembled immediately. As the operator solder the chip, she
> > noticed scale-like defects appearing on the soldemask around the whole
> > stretch of the solder pads. The defects are more prominent on the left
> > side compare to right of the chip. This is repeated for the rest of the
> > 5 chips.
> >
> > Being naughty, she touched the board surface with the soldering iron tip
> > and found on the same spot the same defect appearing.
> >
> > One more information : defects found on these 2 boards have a much more
> > rough surface compare to other pieces within the same batch.
> >
> > How the information is sufficent for you to provide opinions.
> >
> > Thanks and regards,
> > Wee Mei
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|