TECHNET Archives

January 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Douglas O. Pauls" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 15 Jan 2004 13:49:10 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (83 lines)
I might suggest the following"
Hand solder using a cored wire flux qualified to J-STD-004 type ROL0, with
compatibility demonstrated per J-STD-001C, Appendix B.

Doug Pauls




                      Ken Patel
                      <[log in to unmask]        To:       [log in to unmask]
                      OM>                      cc:
                      Sent by: TechNet         Subject:  [TN] No Clean solder paste note for Telecom/Networking products
                      <[log in to unmask]>


                      01/15/2004 12:22
                      PM
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to Ken
                      Patel






Experts,

If I have to allow my CM to use No Clean solder paste, what kind of note
should I put on assembly drawing (with some kind of qualification
requirement)? Our product is for telecom/networking industry so I rather
specify some kind of qualification requirements (if any) than just write -
use no clean solder paste. I know all pastes are not same and may not be
suitable for certain industry.



I used to put a note on my assembly drawing for hand soldering something
like...



HAND SOLDER FOLLOWING COMPONENTS USING TELCORDIA (BELCORE) COMPLIANT
NO-CLEAN FLUX.



Any help will be appreciated. Thanking you in advance.



Re,

Ken Patel


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2