hi,
i can only come up with one thought at a time, otherwise my mind explodes. here it is.- it's possible that the copper foil has eensy-weensy holes in it that allow resin to flow though it during the pressing and curing of the laminate. this resin acts as a resist during your etching process.
phil
-----Original Message-----
From: Catherine Smith [mailto:[log in to unmask]]
Sent: Tuesday, January 27, 2004 10:15 AM
To: [log in to unmask]
Subject: [TN] Low level shiny copper spots after cupric chloride etching
Hello, can anybody help me please? We are getting low level (up to 5
microns high) copper spots left on inner layer panels after the cupric
chloride etch. It happens on most kinds of laminate. We have put panels
through our chemical clean line and the etch only and the effect is still
there. Leaving out the chemical clean line or pumicing the panels first
still leaves the spots. The surface is shiny copper and sometimes there
appears to be some residue which we believe to be organic from a slight
carbon peak on an EDAX scan. We found some sticky residue on the rollers
in the etcher which we removed, but the problem didn't go away. We run at
4N HCl and 520mV, regenerating with hydrogen peroxide.
Has anyone experienced this before? Did you discover where the organic
residue came from and the best way to remove it?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|