Mike
It's possible to get a CEM 3 laminate (IPC 4101/12) which is described as
blue translucent. I don't know if it's available in the USA but it is
available in Europe. Let me know if you need any more info.
Geoff Layhe
-----Original Message-----
From: Mike Huffman [mailto:[log in to unmask]]
Sent: Monday, January 12, 2004 8:27 PM
To: [log in to unmask]
Subject: [TN] PCB Material
Does anyone have experience with or know a source for 0.8mm thick clear or
blue translucent pcb material?
Thanks in advance.
Mike Huffman ([log in to unmask] )
CID+, IPC Certified Advanced Interconnect Designer
Electrical CAD Manager
Philips Consumer Electronics, BCT Projection TV
PHONE 865-521-3448, FAX 865-540-8021
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
One Philips Drive, P.O. Box 14810, Knoxville, TN. 37914-1810
Private & Confidential:
This e-mail message is confidential and is intended solely for the person or
organisation to whom it is addressed. If the message is received by anyone
other than the addressee please return the message to the sender by replying
to it and then delete the message from your computer.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|