TECHNET Archives

January 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Fri, 9 Jan 2004 14:00:02 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Steve Kelly <[log in to unmask]>
Subject:
From:
Steve Kelly <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (82 lines)
Hi Doug,

Before Xmas I had asked a question on the Technet about cleaning of wire
bondable gold pads. One of the answers I received was to do plasma and after
doing some further research I actually found some articles also recommending
this process.
Regards Steve Kelly



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Friday, January 09, 2004 1:47 PM
To: [log in to unmask]
Subject: Re: [TN] plasma

        Doug:
        Check for leakage. Do a leak check on the chamber. It may have too
much air going in through a seal. .
        Regards,
        Ramon

> -----Original Message-----
> From: Doug Pauls [SMTP:[log in to unmask]]
> Sent: Friday, January 09, 2004 10:35 AM
> To:   [log in to unmask]
> Subject:      [TN] plasma
>
> Good morning all,
>
> I have a question related to plasma cleaning.  We have two plasma
cleaners,
> same model, using Argon-Hydrogen in both, same mixture, same power level,
> but the plasma in one appears more purple than the plasm in the second
> cleaner.  Any ideas as to why?
>
> Secondly, does anyone know if repeated exposure to plasma cleaning will
> degrade the surface of a gold pad and thus reduce bond wire strength?
>
> Thanks.
>
> Doug Pauls
> Rockwell Collins
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2