committee or those committee leaders should have said anything like
that.
The committee has been gathering lots of info about LF and that content
is one of the primary drivers of the next Rev; also for J-STD-001D.
Current draft only has a placeholder but planning on major work to
finally build the section at the coming APEX meeting Feb 22-23 in
Anaheim.
610D meeting minutes and comments
http://www.ipc.org/committeedetail.asp?Committee=7-31B
Draft link: http://files.ipc.org/R610D_Feb04.zip
Jack Crawford
Director, Certification and Assembly Technology
[log in to unmask]
847-790-5393
fax 847-504-2393
-----Original Message-----
From: Shelton, Megan [mailto:[log in to unmask]]
Sent: Friday, January 30, 2004 12:58 PM
To: [log in to unmask]
Subject: Re: [TN] IPC-610 Rev D
maybe an amendment add because we all need to know this
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Kathy Kuhlow
Sent: Friday, January 30, 2004 1:15 PM
To: [log in to unmask]
Subject: [TN] IPC-610 Rev D
I was at a seminar yesterday and the topic was lead free. The statement
was
made that the Rev D 610 will not be changed to address the solder joint
criteria for lead free processing.
Jack - is this true? If so, why? What is the plan for implementation
into
the 610 acceptance criteria?
Kat
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|