I would say no. Most solder masks and laminates are highly resistant to
isopropyl. Part markings or non-epoxy marking inks could be an issue. How
long is the soak? Unless it is for hours on end, I would not expect
problems. I would make sure the alcohol had flashed off and baked off
before the next process step.
Doug Pauls
"Schleman, Joe
A." To: [log in to unmask]
<[log in to unmask] cc:
OM> Subject: [TN] Soaking Circuit Boards in Alcohol
Sent by: TechNet
<[log in to unmask]>
01/23/2004 10:40
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to
"Schleman, Joe
A."
Hi,
I happened to observe somebody soaking some assembled boards in isopropyl
alcohol to clean them. I was wondering if this was an acceptable method for
cleaning. I know using alcohol to clean is okay but, I'm not so sure about
actually soaking the whole assembly in an alcohol bath. Any Insight would
be
appreciated. Thanks.
Joe
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|