Joe,
Have you looked into Titanium? I did a Google search on "2-56 titanium
screws" and it came up with several suppliers.
I've tried Teflon coating over stainless for repeated wave soldering
applications and it doesn't last long. If you feel you should give it a try,
I recommend "Tiodize" in Huntington Beach, Ca. 714-898-4377
BTW, I went to High School with a Joe Kane in N.J. Might you be him?
Regards,
Ed Popielarski
QTA Machine
27291 Jardines
Mission Viejo, Ca. 92692
Phone:949-581-6601
Fax: 949-581-2448
WWW.QTA.NET
"Thank God for America...
before it's too late!"
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|