Thanks to all for the responses. Your opinion confirmed my initial reaction when I saw this as the mid-term solution to a MSD issue.
Don Vischulis
-----Original Message-----
From: [log in to unmask]
Sent: Jan 15, 2004 9:53 AM
To: [log in to unmask]
Cc: [log in to unmask]
Subject: Re: [TN] MSD Question
Hi Don! Here's a quick answer - if the Sn/Pb component finish is not
sufficiently thick you will run the risk of degrading the solderability -
the higher the bake temperature the quicker/greater the degradation. Good
Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Donald Vischulis
<dvischulis@earth To: [log in to unmask]
link.net> cc:
Sent by: TechNet Subject: [TN] MSD Question
<[log in to unmask]>
01/14/2004 08:26
PM
Please respond to
Donald Vischulis
Just a quick question: What is your opinion of a MSD control procedure the
requires baking tin/lead terminated (coated) components every 7 days?
Don Vischulis
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------