TECHNET Archives

January 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"Arbour, Michel" <[log in to unmask]>
Date:
Wed, 14 Jan 2004 12:55:25 -0500
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Arbour, Michel" <[log in to unmask]>
Parts/Attachments:
text/plain (28 lines)
Hello technet,
One of our customer reported a problem with a lot of battery but we are
confused as how to interpret the results.
The battery if a full metal casing with the negative lead spot welded to the
casing while the pos. lead connects inside.The visual aspect of the leads
are excellent.
The test consists to dip the component in a stainless steel ultrasonic bath
containing de-ionized water at 70C. The part is lying on a nylon net.
The positive lead of the battery gets darkened after 5 minutes in this bath.
Only the positive pin gets dark (oxydized)

Are we in the presence of an electrolytic reaction??
Is it contamination of the positive lead that cause this reaction ?
Any other test to suggest ?

Regards
MIchel Arbour

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2