Interesting thanks.
If you do survey suppliers and they reply, (don't forget all the world
and his brother is writng to them on this so they might be a bit
overwhelmed), I think you will find that a large number of passive
suppliers are already using Sn as a finish, whether devices are marked
Pb-free or not.
I say whether they reply or not as I recently attended an in-company
Pb-free day. The host advised that they had simply asked suppliers if
they had a Pb-free plan and who was in charge of it. Less than 1 in 3
responded. And only a half of those were positive. I suppose you have to
assume that the rest did not have a plan....
Regards
Mike Fenner
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, December 10, 2003 4:44 PM
To: [log in to unmask]
Subject: [TN] Components Suppliers who are using Tin Finishes
Hi All!
I've been asked by one of our sales folks what we are doing to try and
prevent the problem of Tin whiskers from occuring on the products that
we build...apparently he was asked that from a potential customer.
I've been doing some researching and studying the topic through net
searches and whatnot, and found a good paper at:
http://www.calce.umd.edu/lead-free/tin-whiskers/TINWHISKERMITIGATION.pdf
One of the things it said to do was to determine if any of the component
suppliers that you use, are using or considering using Tin finishes.
Does anybody know of a listing somewhere that shows what finishes
component suppliers are using? Or does one have to just call and ask
each one?
Appreciate any information...
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::
This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.
:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|