You can not switch to Lead Free process unless you are 100% sure that all
the components, PCBs, Equipment are comply to this process.
You can work with Tin Lead (63-37 ) in the wave soldering pot an din the
paste for reflow and in the wire for manual soldering and to assemble Lead
free finishing on the components terminations / PCBs.
You may expect increasing in the % of the Tin in the solder pot in such
case.
Best Regards
Reuven
"Blair K. Hogg"
<blair.k.hogg@GAI-T To: [log in to unmask]
RONICS.COM> cc:
Sent by: TechNet Subject: Re: [TN] SnPb Solder pot composition
<[log in to unmask]>
05/12/2003 16:11
Please respond to
"TechNet E-Mail
Forum."; Please
respond to "Blair
K. Hogg"
I was thinking that perhaps a switch from HASL to Immersion Tin could
contribute? If the primary surface is already tin, would the tin
depletion in the solder pot be less?
But then again, if the PCB finish was switched to tin, why would the
process still use solder with lead it in? Going only half lead-free?
>>> [log in to unmask] 12/04/03 08:50PM >>>
Hi Gary,
LTNS!
Perhaps some phenomena associated with a "new" PCB Fab/plating
process?
Any fab or metallurgists out there have a clue?
Have a safe and happy holiday!
Regards,
Ed Popielarski
QTA Machine
27291 Jardines
Mission Viejo, Ca. 92692
Phone:949-581-6601
Fax: 949-581-2448
Cel: 949-337-2578
www.QTA.NET
"Thank God for America...
before it's too late!"
----- Original Message -----
From: "Gary Camac" <[log in to unmask]>
To: "TechNet E-Mail Forum." <[log in to unmask]>; "Ed Popielarski"
<[log in to unmask]>
Sent: Thursday, December 04, 2003 2:13 PM
Subject: Re: [TN] SnPb Solder pot composition
> I would usually agree with Ed's statement on tin content dropping. I
have
many years of Kester Solder Analysis Reports, option C, that support
that
statement. But, for the
> last four months my tin content has ran 63.16, 63.42, 63.24, and
63.4. No
pure tin was added during this period, only virgin solder. Sure has
got me
scratching my head.
>
> Gary Camac
>
> Ed Popielarski wrote:
>
> > Yordan,
> >
> > Deviation from 63/37 can cause increased solder shorts in a wave
soldering
> > machine. At 63/37 (eutectic) the melt point is minimum, and there
is no
> > plasticus range. As you drift from there the melt point increases
and
the
> > plastic range increases. This is why hand solder is preferred at
60/40...
> > there IS plastic range and makes it easier to judge the joint as
you
solder.
> > This is also the main cause of "frosty" joints (I hate to say
"cold"
since
> > it is a very inaccurate term).
> >
> > Another thought to add to the mix is the accuracy of the lab. I
recommend
> > using either Alpha Metals or Kester to do the analysis (Type C
which is
the
> > "whole enchilada" variety) and perhaps to rule out other variables
discussed
> > in other's postings, take a few samples, from the static part of
the
pot,
> > from the wave after running at temperature, etc. If all the samples
come
> > back relatively the same, then you are good to go, but if one or
two
stand
> > out, there could be something worth looking into.
> >
> > Additionally, (yes, another variable) the tin is usually the
element
that
> > drops, not the lead. This has me wondering as well. Why?
> >
> > Have a safe and happy holiday!
> >
> > Regards,
> >
> > Ed Popielarski
> > QTA Machine
> > 27291 Jardines
> > Mission Viejo, Ca. 92692
> >
> > Phone:949-581-6601
> > Fax: 949-581-2448
> > Cel: 949-337-2578
> >
> > www.QTA.NET
> >
> > "Thank God for America...
> > before it's too late!"
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following
text
in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail
to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
http://listserv.ipc.org/archives
> > Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information,
or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> > -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
**********************************************************************
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they
are addressed. If you have received this email in error please notify
the system manager.
This footnote also confirms that this email message has been swept
for the presence of computer viruses.
www.hubbell.com - Hubbell Incorporated
**********************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|