Thanks
Best Regards
ROKAH Reuven
Chief Engineer
ECI Telecom LTD.
Operations Division
30 Hasivim St. Petah-Tikva 49517
ISRAEL
Tel: 972-3-9266734 Mobile:972-55-786734
Fax: 972-3-9266480
e mail: [log in to unmask]
"Dehoyos, Ramon"
<ramon.dehoyos@N To: [log in to unmask]
GC.COM> cc:
Sent by: TechNet Subject: Re: [TN] Conformal coating - PARYLENE DIMER DPX-C
<[log in to unmask]
>
15/12/2003 15:35
Please respond
to "TechNet
E-Mail Forum.";
Please respond
to "Dehoyos,
Ramon"
Reiven:
Pro: Coats everything and seals it.
Con: Slow process, lots of equipment upkeep,
Some board usage needs this type of CC, most do not.
Regards,
Ramon
> -----Original Message-----
> From: TechNet [SMTP:[log in to unmask]] On Behalf Of Reuven ROKAH
> Sent: Sunday, December 14, 2003 2:54 AM
> To: [log in to unmask]
> Subject: [TN] Conformal coating - PARYLENE DIMER DPX-C
>
> Hi Perylene users,
>
> Can you share with your experience and inform the + and - of this
process?
>
> I have last week visited one of the users site and it seems promising.
>
> I have long experience with spraying systems and not vacuum systems.
>
> Best Regards
>
> Reuven
>
>
>
>
> Graham Naisbitt
> <Graham.Naisbitt@CON To:
[log in to unmask]
> COAT.CO.UK> cc:
> Sent by: TechNet Subject: Re: [TN]
Foreign material on top of the conformal coating
> <[log in to unmask]>
>
>
> 12/12/2003 18:02
> Please respond to
> "TechNet E-Mail
> Forum."; Please
> respond to Graham
> Naisbitt
>
>
>
>
>
> Bruce
>
> If you are applying epoxies and other materials after conformal coating,
> just be sure that the solvents (if any) are not affecting the coating
> during
> their application and curing.
>
> Otherwise this should simply be regarded as a cosmetic issue.
>
> Cleaning after all these processes is unlikely to be a good option, as
the
> coating will now be expected to withstand your cleaning process...and
> surface cleaning using brushes, swabs etc., are only likely to be moving
> the
> stuff around on the surface rather than removing it.
>
> Hope this helps
> --
> Regards Graham Naisbitt
>
> [log in to unmask]
>
> Cell: 079 6858 2121
> Office: +44 (0)1252 813706
>
> Concoat Limited - Engineering Reliability in Electronics
>
> NEW - HumiSeal 1H2O Bov Aerosol - NEW
>
> Web: www.concoat.co.uk and www.concoatsystems.com
>
>
> > Hey guys,
> > I have be hit recently on a couple of occasions by the quality folks
> > over "foreign material" that is present on CCA's after conformal
coating.
> > On quite a few boards we install heat sinks after CC and usually use an
> > epoxy to aid in heat transfer as well as loctite on the mounting
screws.
> I
> > have been gigged for the residuals (just smears really) whether it is
on
> > the solder pads or not. I know that we all are concerned with material
> > left over directly on the solder connections, but I am having trouble
> with
> > this one from a logical standpoint. I mean lets face it, you
definitely
> > can't test for the presence of ionic contaminants or anything, but I
know
> > the general impression is the boards should be clean.
> >
> > I know the simple answer here is to clean up all the residuals (and
> > everyone is instructed to do that), but there are times when stuff just
> > happens.
> >
> > Your thoughts
> >
> > Bruce Stilmack
> > GDLS-TO Manufacturing Engineer
> > (850) 574-4773
> > [log in to unmask]
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following text
in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> > Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> > additional information, or contact Keach Sasamori at [log in to unmask] or>
> > 847-509-9700 ext.5315
> > -----------------------------------------------------
> >
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask]
or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|