TECHNET Archives

December 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Wed, 10 Dec 2003 17:53:22 -0000
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (61 lines)
Yes but given that the stuff has been on some components for ever, how
justified is the concern? Do reflowed components, as opposed to as
supplied, whisker and if they do is it significant? One of the ways to
reduce whiskering is thought to be to "anneal" the as deposited coating,
which will happen on the areas not exposed to paste during reflow
soldering. Those areas that are soldered (In wave all outward faces)
will not be pure tin any more.

Regards

Mike



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Wednesday, December 10, 2003 5:50 PM
To: [log in to unmask]
Subject: Re: [TN] Components Suppliers who are using Tin Finishes


Ken,
Simple: its cheap and solders well.  Problems down the road? "Hey not
our concern."  Ah, life is beautiful on the way to the bank. Bev
Christian Research in Motion

-----Original Message-----
From: Bloomquist, Ken [mailto:[log in to unmask]]
Sent: December 10, 2003 12:39 PM
To: [log in to unmask]
Subject: Re: [TN] Components Suppliers who are using Tin Finishes


I have another question along this same subject line.

If everyone is going nuts over "Tin Whiskers" why are the component
manufacturers using tin as an alternative finish to tin/lead? Almost
every stone you turn over, regarding going lead free, you find an
article on "Tin Whiskers". Why not switch to something else that the
industry is not having trouble with???

Ken Bloomquist

:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::

This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.

:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2