TECHNET Archives

December 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 9 Dec 2003 17:36:29 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Thompson, David" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="Windows-1252"
From:
"Thompson, David" <[log in to unmask]>
Parts/Attachments:
text/plain (132 lines)
Brian:  For the record, Panasonic, along with most other TV manufacturers, eliminated lead from the panel glass some time ago.  When we did still use lead in the panel, I understand that it was in the 3% range.  

I am now checking with out glass suppliers to obtain more detailed information and will hopefully be able to provide this soon.

David A. Thompson
Director
Corporate Environmental Department  3G-4
Matsushita Electric Corporation of America
One Panasonic Way
Secaucus, NJ 07094

TEL:  (201) 271-3486
FAX:  (201) 348-7686
NEW ADDRESS: [log in to unmask]

PS  Brian:  Sorry for the duplication.  My original transmission did not go through.


-----Original Message-----
From: Brian Ellis [mailto:[log in to unmask]]
Sent: Tuesday, December 09, 2003 5:22 AM
To: [log in to unmask]
Subject: Re: [LF] Amount of Pb in a "typical" motherboard


Chuck

There are some anomalies in your discussion, IMHO.

I'll go along with you on the funnel (1 -9 lbs), but most of the lead is 
  in the front screen. An 18" screen has a screen size of 36 x 30 cm and 
is about 15 mm thick (monitors are thicker than TVs, as they are used 
closer to the user's face and radiation levels have to be lower). That 
gives a volume of 1,620 cm3. I believe the PbO content of the glass is 
about 30% v/v, = 480 cm3. The density of PbO is ~9 (depends on the 
crystalline form), of which ~90% is lead, so that would give about 4 kg 
or nearly 9 pounds for the screen faceplate alone.

In fact, something like 20% of the weight of a TV or CRT mmonitor is 
lead. Anyone who has handled a 28" TV CRT, without the focus and 
deflection coils knows it is bloody heavy, on its own. The guts are made 
up mostly of very thin nickel sheet metal and have a total weight, 
including the shadow mask, of <100 g. The rest is practically all lead 
glass.

Chuck Dolci wrote:
> Here is some data that the EIA gathered on lead in monitors.
> 
> 3% of US lead consumption is oxides in glass and ceramics (includes CRTs 
> and other uses)
> Reduced to minimum amount for effective x-ray shielding; encased in 
> glass matrix
> Found in 4 major areas of CRT (range 8” - 35” and above)
>        Funnel Glass 1 - 9 lbs
>        Frit (Solder Glass)- 0.057 - 0.215 lbs
>        Panel Glass - used by 25% of industry 0.2 - 2.0 lbs
>        Neck Glass 0.027 - 0.054 lbs
> 
> Range of total lead in CRTs: 1.08 -9.27 lbs
> Average CRT: 18”, 2.16 - 2.59 lbs lead
> 
> I assume TVs have slightly more than monitors because they have tuning 
> and audio circuitry that monitors don't.
> 
> 
> According to "Alternative Technologies for Surface Finishing 
> (EPA/744-R-01-001) June 2001," available at  www.epa.gov/dfe
> lead comprises 0.7% total weight of a typical printed circuit board
> 
> Chuck Dolci
> 
> Hal P Abel wrote:
> 
>> Clark,
>>
>> The big hitter is the CRT monitors. I believe that they contain 10 Lbs of
>> lead.
>>
>>
>>                                                                         
>> Hal
>> Abel
>>
>> -------------------------------------------------------------------------------Leadfee 
>> Mail List provided as a service by IPC using LISTSERV 1.8d
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Leadfree
>> To temporarily stop delivery of Leadree for vacation breaks send: SET 
>> Leadfree NOMAIL
>> Search previous postings at: http://listserv.ipc.org/archives
>> Please visit IPC web site 
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
>> information, or contact Keach Sasamori at [log in to unmask] or 
>> 847-509-9700 ext.5315
>> ------------------------------------------------------------------------------- 
>>
> 
> 
> -------------------------------------------------------------------------------Leadfee 
> Mail List provided as a service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Leadfree
> To temporarily stop delivery of Leadree for vacation breaks send: SET 
> Leadfree NOMAIL
> Search previous postings at: http://listserv.ipc.org/archives
> Please visit IPC web site 
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 
> ext.5315
> ------------------------------------------------------------------------------- 
> 
> 
> 

-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-------------------------------------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2