Doug,
Depends... just kidding!
"Our specifications are based on solder joint connections and the solder specifications are not in question." What does this mean?
What solder joint requirements?
Is epoxy rigidity good or bad? Is it brittle? Is it stronger?
No, I do not know of any public report of the type you are talking about. I would expect some of the big boys have their own internal ones.
Bev Christian
Research in Motion
-----Original Message-----
From: Doug Pauls [mailto:[log in to unmask]]
Sent: December 9, 2003 3:14 PM
To: [log in to unmask]
Subject: [TN] Adhesive strength vs overhang
Good afternoon all,
Internally, we are having discussions on the amount of allowable overhang
of passive SMT components (R and C). Our specifications are based on
solder joint connections and the solder specifications are not in question.
We have an application where a silver filled adhesive is used to make the
connection between SMT metalization and mounting pad. The solder joint
requirements were applied to these adhesive joints and I am wondering as to
the validity of this. The adhesive is epoxy based and, in my mind, more
rigid than solder. I think we are unnecessarily rejecting parts that are
acceptable.
So, before I go off and do a complex designed experiment, I thought I would
check with the Technet crowd first. Do you know of any studies that show
the adhesive force (e.g. pull strength) vs. the degree of pad overhang?
Doug Pauls
Rockwell Collins
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|