Hi Steve,
What we are finding is that each component manufacturer has to go through a
qualification procedure for each lead-free finish they use.
We are finding that most manufacturers have chosen only one lead-free finish
(some have two available) for each package family.
I have seen 100% tin finish on resistors, capacitors, SOICs, PLCCs, MLFs,
and QFPs, among others.
Sincerely,
Debbie Goodwin
Account Representative
10867 Portal Dr
Los Alamitos, CA 90720
Phone = (714) 252-0010
Fax = (714) 252-0026
[log in to unmask]
PLEASE NOTE - Over 90% of all SMT packages are now available Lead-Free!!!
__________________________________________________
This message is intended for the use of the individual entity to which it is
addressed and may contain information that is privileged, confidential and
exempt from disclosure under applicable law. If the reader of this message
is not the intended recipient, or the employee or agent responsible for
delivering the message to the intended recipient, you are hereby notified
that any dissemination, distribution or copying of this communication is
strictly prohibited. If you have received this communication in error,
please notify us immediately by calling
714.252.0010 or returning the original message to us. Thank You.
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Wednesday, December 10, 2003 8:44 AM
To: [log in to unmask]
Subject: [TN] Components Suppliers who are using Tin Finishes
Hi All!
I've been asked by one of our sales folks what we are doing to try and
prevent the problem of Tin whiskers from occuring on the products that we
build...apparently he was asked that from a potential customer.
I've been doing some researching and studying the topic through net searches
and whatnot, and found a good paper at:
http://www.calce.umd.edu/lead-free/tin-whiskers/TINWHISKERMITIGATION.pdf
One of the things it said to do was to determine if any of the component
suppliers that you use, are using or considering using Tin finishes.
Does anybody know of a listing somewhere that shows what finishes component
suppliers are using? Or does one have to just call and ask each one?
Appreciate any information...
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|