Ron, Louis, Dale, Edward, Hans, Ramon, Sasha, (hope didn't miss anyone)
thank you all for the inputs! The analysis was done by means of a scanning
electronic microscope JEOL JSM 35 CF with X-ray microanalyser TRACOR
NORTHERN TN-200, and for samples are used JEOL standards. Parallel to this
we have order an analysis of new solder 63/37 (a kind of reliability check)
and it showed Sn - 62,37%/ Pb-37,62%. As far as the other materials (Cu, Au,
Sb, Fe, Al, Zn) are concerned it seems we have very low level of
impurities - below 0.01%. Besides the missing Antimony in our analysis, are
there other impurities with crucial impact on the solder quality that must
be checked? Sasha, unfortunately, the still surface of the pot while taking
sample is not the case - the sample was drown after the solder was mixed
well and from the "crest of the wave".
Yordan
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Edward Szpruch
Sent: Wednesday, December 03, 2003 4:47 PM
To: [log in to unmask]
Subject: Re: [TN] SnPb Solder pot composition.
Yordan,
I do have experience with solder wave, only with HASL, but I presume the
rules are the same:
-usually the analyses is done to indicate more than 10 materials such as
Copper, Gold, Antymony, Iron,Silver etc.Those have high influence on both
metling point and solder joint quality.Limits on such material are really on
low level.
- Concerning Pb - Sn : usually only one of them is analysed, the second
stated by ballance to 100% .
The results concerning Pb-Sn are OK, but what with other stuff???
Edward
> -----Original Message-----
> From: Louis Hart [SMTP:[log in to unmask]]
> Sent: ד דצמבר 03 2003 16:25
> To: [log in to unmask]
> Subject: Re: [TN] SnPb Solder pot composition.
>
> Yordan, I'll leave others to comment on solder joint quality and
> reliability. How are the composition analyses done? I'd bet the
> measurements are not truly good to 0.01%. I asked a big solder
> manufacturer
> for measurement quality data 2 or 3 years ago, and did not get a good
> answer. Lou Hart
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Yordan Venev
> Sent: Wednesday, December 03, 2003 7:58 AM
> To: [log in to unmask]
> Subject: [TN] SnPb Solder pot composition.
>
>
> We have made a composition analysis of our solder wave solder pot and
> discovered a deviation of the SnPB content. The Sn percentage had gone up
> to
> 65.45% and the Pb content down to 34.54%. I suppose there will be a
> (small)
> change in the constitutional behaviour of the alloy - some bigger range of
> the liquid-to-solid stage. Except this, what should we be aware of in
> practice in regards to solder joint quality and reliability? We continue
> to
> maintain the pot temperature at 250 deg C (482 deg F).
>
> Any inputs will be appreciated!
>
> Best regards,
> Yordan Venev
>
> ********************************************************
> CENTILLION LTD.
> 7-th km Tzarigradsko shosse Blvd.
> ATM Center
> 1784 Sofia, BULGARIA
> Tel. :(+359 2) 974 47 51, 965 84 95, 965 58 85
> Fax :(+359 2) 974 47 52
> mail to: [log in to unmask]
> www.centillion-bg.com
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|