Hello Ken,
If I understand the question, the answer maybe:
IPC-9252 'Guidelines and Requirements for E.T. Unpopulated Printed Boards'.
Section 4.3, Table 4-1 'Test Requirements by Level'
Class 3,continuity 50 ohms, pass 0 to 50, fail > 50 ohms.
I hope this helps.
Paul Holloway
-----Original Message-----
From: Crepeau, Phil [mailto:[log in to unmask]]
Sent: Tuesday, December 02, 2003 12:35 PM
To: [log in to unmask]
Subject: Re: [TN] Continuity requirement (resistance value) for class 3
product
hi ken,
i'm afraid i don't understand your question. could you expand on this?
thanks,
phil
-----Original Message-----
From: Ken Patel [mailto:[log in to unmask]]
Sent: Tuesday, December 02, 2003 8:57 AM
To: [log in to unmask]
Subject: [TN] Continuity requirement (resistance value) for class 3
product
Technetters,
What is the current Continuity requirement (resistance value) for class 3
product at bare board level?
Re,
Ken Patel
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|