TECHNET Archives

December 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Marsico, James" <[log in to unmask]>
Date:
Wed, 10 Dec 2003 08:37:39 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Phil Nutting <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Phil Nutting <[log in to unmask]>
Parts/Attachments:
text/plain (82 lines)
James,

This may not be a viable solution, but for years my father-in-law used Vaseline on all his electronic connections on his boat which was in a salt water environment.  He never loss radio communication or had lighting issues.  Yes is can be messy, but when things get rotten it is nice to know your radio will still work.  A Silicon grease might be a more modern day material to use. Neither of these are Manufacturing solutions I would rush out to use, but maybe they can point to something simple rather than complex.

Phil Nutting

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Marsico, James
Sent: Wednesday, December 10, 2003 7:28 AM
To: [log in to unmask]
Subject: Re: [TN] GOOD RF GROUND


This specific application doesn't warrant a Teflon substrate, I think it is
FR-4.  Let me clarify one thing, It's assumed that the material is cold
flowing, causing ground interruptions (this is an RF Engineer's assumption).
The fact is that, after time in service, the main complaint from the test
guys is electrical problems associated with a degenerated ground.  It could
be associated with moisture entering the housing causing the tin-lead
plating on the ground plane, which is in direct contact to the housing via
screws, to become slightly oxidized.  This is not a hermetically sealed
housing.  In fact, there is a hole in it to allow for a pot adjustment.
Which leads to another question...  are there bulk-mounted pots available,
mounted directly to the housing wall, which would eliminate the hole?

Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879


        -----Original Message-----
        From:   Crepeau, Phil [SMTP:[log in to unmask]]
        Sent:   Tuesday, December 09, 2003 4:47 PM
        To:     [log in to unmask]
        Subject:        Re: [TN] GOOD RF GROUND

        hi,

        is the fastener loosening up because the laminate is teflon based
(which is common in rf applications)?

        phil

        ---------------------------------------------------
        Technet Mail List provided as a service by IPC using LISTSERV 1.8e
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
        To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
        Search the archives of previous posts at:
http://listserv.ipc.org/archives
        Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
        -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2