Mario,
Even though this is a rejectable condition, with the customers
blessing we have MRB'd (agreed between Mfg, Quality and Eng.) that this is
a usable condition on many occasions. The conformal coat will more that
protect the area from corrosion concerns and will also isolate the area.
BS
Mario Dion
<mdion@MEDIAT To: [log in to unmask]
RIX.COM> cc:
Sent by: Subject: Re: [TN] Assembled pcb with exposed copper; is
TechNet conf.coating appropriate to "isolate" the exposed
<[log in to unmask] copper ?
ORG>
11/07/2003
09:11 AM
Please
respond to
"TechNet
E-Mail
Forum.";
Please
respond to
Mario Dion
Bonjour Leo,
Thanks for your input. I was aware that it is a rejectable condition but
since there is $$$ involved if we have to scrap the ccas then that explain
why I was looking for a viable solution.
By the way, my house is brand new so I can't check for the copper plumbing
which anyway are made out of plastic tubbing... ;o)
See you in Amherst on December !
Have a great week end all,
Mario
-----Original Message-----
From: Leo Lambert [mailto:[log in to unmask]]
Sent: 7 novembre, 2003 09:00
To: TechNet E-Mail Forum.; Mario Dion
Subject: RE: [TN] Assembled pcb with exposed copper; is conf.coating
appropriate to "isolate" the exposed copper ?
Interesting, the boards are hot air leveled (HAL), if inspected to
IPC-A-600, sect 2.4.1 Nonwetting, states that this is a non conforming
condition for all classes of products, Class 1, 2, 3,. The issue being, if
the boards are hot air leveled and there is exposed copper means that non
wetting is occurring and this is not acceptable. The basis material is
exposed and it is not supposed to be exposed.
IPC-A-610, the assembly document states in sect 6.5.6 Nonwetting that this
is a defect for Class 1, 2, 3, if solder is required. Since this board is
HAL, solder is required and therefore it again does not meet the
requirements of the specification.
So my opinion at this point is that the board is rejectable.
Now for the reality. Exposed copper will not cause you a problem, many
products have been built through the years with exposed copper, if not on
the ends of the component leads, along the edges of all the conductor
traces. And by the way go check your plumbing in your house and let me know
how your copper pipes are doing after all these years. We also have boards
that are OSP protected, once these boards are soldered the OSP coating is
for all practical purposes gone, so you have exposed copper all over the
board if the solder did not wet to the edges of all the pads. Some
companies
have been building boards like this for over 20 to 25 years.
What to do? Identify the condition as a defect due to it does not meet the
specification, work with your subcontractors to get their act together, and
disposition the boards to use as is.
That's my cut at it. Will be interested to hear what others have to say.
Leo Lambert
Technical Director
EPTAC Corp
[log in to unmask]
www.eptac.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Mario Dion
Sent: Thursday, November 06, 2003 5:10 PM
To: [log in to unmask]
Subject: [TN] Assembled pcb with exposed copper; is conf.coating
appropriate to "isolate" the exposed copper ?
Bonjour Technetters,
Would a pcb assembly with exposed copper around some vias be reliable if
fully coated with conformal coating so copper won't be exposed anymore ?
The problem was not detected at the incoming inspection so many pcb were
assembled. Board finish is HASL.
Thanks for your comments,
Salutations,
___________________________
Mario Dion, T.Sc.A./ A.Sc.T.
Production Engineering
Mediatrix Telecom Inc.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|