Doug,
I was also going to suggest the floating balls (nylon, or polypropylene I believe), ala plating baths. I think that I have seen them in either McMaster-Carr, or Grainger as well.
I believe that at one point, someone used ping-pong balls, but don't think they would hold up to well in toluene.
Steve
-----Original Message-----
From: Doug Pauls [mailto:[log in to unmask]]
Sent: Wednesday, November 12, 2003 4:37 PM
To: [log in to unmask]
Subject: [TN] Sponges and Toluene
Anyone know of any sponge material that is resistant to toluene? I have a
spray application where the spray heads, to avoid gumming up, are immersed
in toluene. This leads to a fairly large evaporation. My thought was that
a sponge material would keep the heads wet with toluene, but would minimize
evaporative loss. I am open to suggestions.
Doug Pauls
Rockwell Collins, where toluene and Mt. Dew lead into previously unexplored
territory..........
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|