TECHNET Archives

November 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
Date:
Thu, 20 Nov 2003 07:22:00 -0500
Content-Disposition:
inline
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Tom Gervascio <[log in to unmask]>
Subject:
From:
Tom Gervascio <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Sender:
Parts/Attachments:
text/plain (14 lines)
We are considering using an automatic system to monitor and control additions of a saponifier to our Electrovert H400+ wash. Any recommendations on systems that other's have used? Any trade-offs on closed loop monitoring systems using pH versus refractometer? I thought that if you use water soluble masks that the dissolved materials might influence the dissolved solids measured with refractometer. However it seems that drag out with normal operation approaches 7 gal/8 hour shift. with a prewash and wash capacity of 95 gallons this means that over 12 shifts that the wash should be turned over but I suspect that all the material may not be turned over due to dead spots in the construction of the wash (i.e. 2" level in wash below a U joint that connects the prewash to the wash section). That said is location of the sensors critical- i.e. place them in these areas where the wash may be stagnant or items may settle to the bottom of tanks and heaters.

Thanks for the input

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2