Technetters,
Under the Visual Examination para in IPC-600, IPC-6012, & IPC-6013 reference is made to "1.75x magnification (approx. 3 diopters)". Do any IPC or other Internationally recognized standards list the formula for determining magnification or a table of magnification vs. diopter? When I talked to my vendors and distributors about this topic almost all of them had a different theory and or method for calculating magnification.
Under the Visual Examination para in IPC-610, as the size of the feature being inspected is reduced in size, the magnification increases. One of the magnification powers called out is 4X. Our stereo-microscopes start at 7X or 10X and we do not want to use pocket comparators or jewelers eye loops to perform inspection operations. Does anyone know where 4X halo lamps can be purchased?
Does anyone know of a way to confirm the magnification of a standard Halo lamp?
Vendor references can be sent to
[log in to unmask]
Any and all assitance with this issue is greatly appreciated.
Sheila Akins
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|