The preheating of the whole assembly:
(1) prevents thermal shock, which can cause warping due to large internal
temperature gradients,
(2) prevents large temperature differences between various parts of the
assembly, which also can cause warping (bi-metal strip effect),
(3) reduces the time the assembly needs to be exposed to the solder wave in
order to get good PTH fill,
(4) flux needs to activate and start its work prior to reaching the wave, and
more.
Regards,
Werner Engelmaier
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|