TECHNET Archives

November 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Dehoyos, Ramon" <[log in to unmask]>
Date:
Tue, 18 Nov 2003 06:13:13 -0800
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (70 lines)
        Werner:
                Is the coefficient of expansion for ceramic components
linear or exponential? If it is exponential, components may reach a point
where the expansion still exists but it is negligible. What are your
thoughts?
                Regards,
                Ramon

> -----Original Message-----
> From: Werner Engelmaier [SMTP:[log in to unmask]]
> Sent: Monday, November 17, 2003 10:05 PM
> To:   [log in to unmask]
> Subject:      Re: [TN] Not that our process is out of control or anything,
but --
>
> In a message dated 11/17/2003 16:52:11, [log in to unmask]
writes:
> >It is the preheat it the wave that is controlled (the infamous 2C/sec)
> >to prevent thermal shock.
> ---This is correct.
> >Once the chip has achieved a specified temp, all the materials have
expanded
> equally and >after this point the rapid thermal change of hitting the wave
> does not affect the chip.
> ---Sorry, but there is no such condition; different materials will always
> have a differentiasl thermal expansion, unless they have identical CTEs.
> >It is the different expanding properties of the two materials that cause
the
> chip
> >to crack.
> ---Quite correct.
> >Once they have both expanded to their maximum state, the temperature
curve
> is irrelevant.
> ---Sorry again, but there is no such state; as long as you raise the
> temperature materials will expand, unless they have a negaqtive CTE.
>
> Regards,
> Werner Engelmaier
> Engelmaier Associates, L.C.
> Electronic Packaging, Interconnection and Reliability Consulting
> 7 Jasmine Run
> Ormond Beach, FL  32174  USA
> Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
> E-mail: [log in to unmask], Website: www.engelmaier.com
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2