Edward:
You are SO right, when questioning the thoroughness of testing of boards made in a world where price seems not just the most important thing, but frequently, the ONLY thing that matters.
However, all such questions had to be answered when switching from the old black tank oxide, to the new conveyorized alt oxides, and they can be answered again.. and should be, but someone must be willing to say, "Yes, if the new process passes these tests, I want to look at it...and we do not even get much of that..., sadly."
Rudy Sedlak
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|