TECHNET Archives

November 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 14 Nov 2003 15:00:59 +0100
Content-Disposition:
inline
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "d. terstegge" <[log in to unmask]>
Subject:
MIME-Version:
1.0 (Generated by Clearswift ES version 4.8.1.149)
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII
From:
"d. terstegge" <[log in to unmask]>
Parts/Attachments:
text/plain (29 lines)
Hi Technet,

http://www.parallax.com/images/prod_jpg/bs2p24-ic.jpg is a picture of a
tiny pcb assembly that can be wavesoldered onto a motherboard almost
like a normal through-hole package.  Due to an obsolescense problem we
are thinking about replacing a 22-pins DIP-package by a construction
similar to what's in the picture.
Does anyone know what technology to use to get the sidepins connected
to the substrate, and does this fit within a normal PCB Assembly
process? Also any  ideas about alternative solution are more then
welcome.

Best regards!

Daan Terstegge
Thales Communications
Unclassified mail
Personal Website: http://www.smtinfo.net

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2