Happy, the contact for lead free HASL was/is Greg Bartlett, at Teledyne
HALCO. He spoke at IPC Alternate Final Board Finishes Committee in 2001 for the
Lead Free HASL Users Group. Phone I have for Greg is 603-889-6191, ext 239.
E-mail I have for Greg is [log in to unmask]
My understanding is that problems of putting lead free solders in a HASL
machine had been pretty well worked out. Seems to me they were dross formation,
attack on stainless steel, etc. Of course, operation had to be at a hotter
temperature than eutectic solder.
Denny Fritz
MacDermid
Chair of IPC Alternate Final Board Finishes Solderability Test -5-23d
******************************
Subj: [TN] Lead-free HASL
Date: 10/30/03 9:02:01 AM Central Standard Time
From: [log in to unmask] (Happy Holden)
Sender: [log in to unmask] (TechNet)
Reply-to: [log in to unmask] (TechNet E-Mail Forum.), [log in to unmask]
To: [log in to unmask]
We have a customer asking for Pb-free HASL. I am not familiar with this
finish. The temperature for Pb-free solder would be quite high and the
effects on a board, as well as the HASL equipment might be detrimental.
The customer says it is used in Japan, he quotes a Matsushita Electric
news release. The release seems to indicate that they are using a
lead-free solder paste but that word is not used, just "PCBs with
lead-free solder". Does anyone know of a Pb-free HASL process?
Happy Holden
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|