Linda, we use something that looks like a bent up "shrimp fork".
The flat measuring end is .030" thick and the handle is about 1 1/2" long.
The measuring end has a notch that can be placed over the lead and the wire can be cut to nearly .030". Kind of looks like a lazy "L". \_
Works for us!
Hope this helps.
Ron Dieselberg
Trainer
CMC Electronics Cincinnati
[log in to unmask]
-----Original Message-----
From: Linda Langley [mailto:[log in to unmask]]
Sent: Wednesday, October 29, 2003 9:43 AM
To: [log in to unmask]
Subject: [TN] measuring tool
Technetters,
What type of measuring device do you use to check proper lead length? We
need something to measure .030 on production line. We are currently using 6
inch. Metal ruler but need something a little more accurate.
Thanks for any suggestions.
Linda
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|