Hi John-
Here is a snippet of ROSA.
ACI offers solderability restoration services by using Reduced Oxide
Soldering Activation (ROSA) technology to remove the oxide layers from
circuit boards or components and then re-tin or otherwise coat them to
maintain a solderable surface.
The ROSA technology uses electrochemical reduction principles to convert
surface oxides of a variety of surface finishes, thus restoring
solderability. This process is performed in an aqueous solution so any
residues are easily and quickly rinsed away.
If you are interested please contact Greg Wood or Guy Ramsey
[log in to unmask]
[log in to unmask]
610-362-1200
www.aciusa.org
Enjoy,
Cal Driscoll
Communications Test Design, Inc.
www.CTDI.com
-----Original Message-----
From: John Foster [mailto:[log in to unmask]]
Sent: Friday, October 17, 2003 2:14 PM
To: [log in to unmask]
Subject: [TN] Question about wetting
I have a large inventory of trim capacitors that have exceeded the
manufacturers shelf
life by 2 years. Solderability testing has revealed inadequate wetting. The
parts are on
tape and reel. The plating is a thin layer of tin over nickel. We believe we
have a oxidation problem. Does anyone have any ideas AT ALL on how we can
recover these
parts. The part has gone obsolete I have 86,000 of these things that I
really really need to use.
Any help would be appreciated
Thanks
John Foster
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|