I think the problem is that knowing how much Pb is where doesn't really
give a route map to its elimination, so nobody has thought in this way.
The usual suggested route, in outline, is:

1) Change board finish to eliminate Pb (example: from HASL to Ag or OSP
etc)
2) Wait for component people to bring out lead free and lead free
(temperature) rated devices
3) Change the paste/solder.

In parallel/off line
4) Audit component suppliers for Pb-free availability dates types etc.
5) Pb-free paste/solder can be used now to evaluate approve types,
explore production parameters, gain experience, verify reliability and
so on.

This way ensures compatibility and gives a "change one thing at a time"
path. 1) and 2) are to your specification, but most people have no
control over 2, and availability of components is the real decider on
switching.

Regards

Mike Fenner

Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of d. terstegge
Sent: Monday, October 13, 2003 10:31 AM
To: [log in to unmask]
Subject: [TN] How to estimate the amount of lead in a PCB-Assembly ?


Hi Technet,

I posted this same message to the LeadFree forum last week, but didn't
receive any usefull answers (except a mentioning of the availabliity of
Pulverization & Analytical Techniques), so I try again here :

I just received a question from one of our customers, asking how much
lead their products contain. The answer will help them to make decisions
about changes to their (future) boarddesigns. This seems not so easy to
answer, as lead is introduced in the product as HASL, as solderpaste, as
wave soldered joints and as finishing of component terminations. I don't
want to reinvent the wheel, therefore I'm looking for recommendations on
a practical approach to deal with this question, that I'm sure many of
you have had before. All input is appreciated.

Daan Terstegge
Thales Communications
Unclassified mail
Personal Website: http://www.smtinfo.net

:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::

This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.

:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2