ASTM D 790 TEST METHODS FOR FLEXURAL PROPERTIES OF UNREINFORCED
AND REINFORCED PLASTICS AND ELECTRICAL INSULATING
MATERIALS
For a 3 point bend test on plastics. I think it also gives a reference
to a 4 point test.
Don't know about the other ones.
Good luck,
--
Eric Christison
Mechanical Engineer
STMicroelectronics
33 Pinkhill
Edinburgh
EH12 7BF
tel: +44 (0)131 336 6165
fax: +44 (0)131 336 6001
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------