Hi Eddie,
IPC/EIA J-STD001C asks for removal of gold from (through-hole)
component leads when the thickness of the gold layer is above 2.5
microns, to prevent problems with embrittlement. Thickness on an ENIG
board is typically around 0.05 micron, resulting in a gold content in
the joints far below what's considered dangerous. Perhaps a mouseclick
on "conductor finishing" on the mainpage of my http://www.smtinfo.net
site will get you some better info.
Best regards,
Daan Terstegge
Thales Communications
Unclassified mail
>>> Eddie Rocha <[log in to unmask]> 10/06/03 11:51pm >>>
Does anybody have data or literature which shows that solder joint
embrittlement is not an issue when ENIG is used? I have a customer
that needs this supporting data before he can allow us to use ENIG. Is
this embrittlement issue related only to a certain thickness of gold?
I'd appreciate any feedback on this topic.
thanks,
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|