Hi Brian,
Phoenix x-ray presented to the 610 technical committee last week in MN. The
presentation included the concept of a tab added to the pad geometry to
support Automated X-Ray evaluation of BGA wetting. The idea as I see it is
to see if a graduated fillet occurs on the tab which can be observed through
x-ray evaluation. Seemed reasonable and the illustrations used in the
presentation supported the concept well.
I didn't see much discussion of the process on the web but try:
www.phoenix-xray.com
Best regards,
Mel Parrish
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Smith, Brian
(bsmith37)
Sent: Monday, October 06, 2003 12:23 PM
To: [log in to unmask]
Subject: [TN] Non Round BGA Pads
Good afternoon all. Could anyone out there point me towards some
articles/papers on using non-round
pads for BGAs to improve X-ray inspection? So far all I have been able to
find
are vague hints from Bell Labs or
IBM, but nothing substantial.
Thanks in advance!
Brian Smith
AMT
GCSD Harris Corporation
321-729-3808 (p) 321-729-7348 (f)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|