TECHNET Archives

October 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Henry Rekers <[log in to unmask]>
Date:
Fri, 31 Oct 2003 18:16:04 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Douthit <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii; x-mac-type="54455854"; x-mac-creator="4D4F5353"
From:
David Douthit <[log in to unmask]>
Parts/Attachments:
text/plain (44 lines)
Henry,

Fix the problem!! Get a different connector!
Do not try to "mask" a poor product with a band aid.

Corrosion inhibitor grease/liquids/sprays generally cause more problems then they solve.

David A. Douthit
Manager
loCan LLC

Henry Rekers wrote:

> Has anybody out there had experience with using corrosion inhibiting grease in smt connectors?
>
> I have one connector in particular that causes us troubles.  Specifically where vibration causes the plating of the connectors to be worn off.  I've heard that you can apply a dielectric grease to help this.
>
> Any ideas?
>
> Thanks.
>
> Henry J. Rekers
> Manufacturing Engineer.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2