Paul,
For hi-rel applications,we believe that if you can't clean the vias,you need
to fully plug or tent both sidesof the via.There is nothing in between.You
must choose a robust process for tenting,because you can never allow an
open.You don't know when it happened so you don't know what may be lurking
in yonder walls.
Dewey
> -----Original Message-----
> From: Paul Baine [SMTP:[log in to unmask]]
> Sent: Friday, October 24, 2003 7:31 AM
> To: [log in to unmask]
> Subject: [TN] Cleaning of via holes under components
>
> Hello,
>
> One of our Design Engineers is designing a surface mount PCB
> assembly and would prefer not to have the via holes solder mask
> tented. However, he is concerned that, if he does not call up
> solder mask tenting on his bare PCB drawing, foreign matter could
> find its way into a via hole and, if a component (e.g. an IC) was
> mounted over the via hole, the foreign matter might not be removed
> during the cleaning process.
>
> Has anyone had experience with this situation? I would appreciate
> any help you could give me.
>
> Thanks very much in advance.
>
> Paul Baine
> Q.A. Manager
> C-Tech Ltd.
> Cornwall, Ontario, Canada
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|