TECHNET Archives

October 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Franklin D Asbell <[log in to unmask]>, "TechNet E-Mail Forum." <[log in to unmask]>
Date:
Thu, 23 Oct 2003 12:33:06 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Morse, Carrie" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Morse, Carrie" <[log in to unmask]>
Parts/Attachments:
text/plain (28 lines)
I'm actually looking for one for Assembly -- IPC-A-610C.  But....Frank...
If you have one for Bare boards we can use it as a template and add the assembly info.

Thanks!
-Carrie

-----Original Message-----
From: Franklin D Asbell [mailto:[log in to unmask]]
Sent: Thursday, October 23, 2003 12:43 PM
To: TechNet E-Mail Forum.; Morse, Carrie
Subject: Re: [TN] IPC Defect vs. Root Cause Matrix


I've got one for bare printed circuit boards...is this what you're looking
for, or for assembled product???

Franklin

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2