TECHNET Archives

October 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Eric Laroche <[log in to unmask]>
Date:
Thu, 2 Oct 2003 07:04:09 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (146 lines)
                DPMO is defects per million opportunities. Lets say that 97
boards were fully assembled.  Each board has 2875 opportunities. It makes a
total of 278875 opportunities for all the boards. All the defects were added
and they were 349.
        278875 times 3.5858 is one million. Multiply 349 times the previous
number and it results is 1251 DPMO.
                The opportunities can be obtained from the cad data and
there are software that can compute, graph, plot per type of board,
operation, shift, and so on. Also there are books that explain this more in
detail. Took a course long time ago and got used to the software do all the
work. What I explained is an abbreviated form of how it works. 
                Regards,
                Ramon

> -----Original Message-----
> From: Eric Laroche [SMTP:[log in to unmask]]
> Sent: Thursday, October 02, 2003 9:34 AM
> To:   [log in to unmask]
> Subject:      [TN] RE : [TN] DPU and PPM
> 
> Ramon,
> 
> Can you expand a little on DPMO?  What is measure and how is it
> calculated?
> 
> Thanks
> 
> Eric
> 
> -----Message d'origine-----
> De : TechNet [mailto:[log in to unmask]] De la part de Dehoyos, Ramon
> Envoyé : 2 octobre, 2003 09:17
> À : [log in to unmask]
> Objet : Re: [TN] DPU and PPM
> 
>         Howard:
>                 It depends on the complexity of the board. It could be
> 0.7,
> 1.9 or 3.5.  One board can have two defects others can have 7 defects
> and
> some none. DPU is a defect average of many boards of the same type.
> DPUs
> can be compared with other groups of boards of the same type.  Gauging
> the
> whole shop for quality, a better method can be used, which is DPMO.
> Using
> DPMO all the boards can be put in the metric.  Every part that gets
> placed
> by the chip shooter or the pick and place, every solder joint are
> opportunities.  A DPMO of under 1000 is a good number in my point of
> view.
> Under 500 is great.
>         Regards,
>         Ramon
> 
> 
> > -----Original Message-----
> > From: Howard Watson [SMTP:[log in to unmask]]
> > Sent: Wednesday, October 01, 2003 5:22 PM
> > To:   [log in to unmask]
> > Subject:      [TN] DPU and PPM
> >
> >
> > Hi everyone,
> >
> > The upper management team here uses a DPU metric for our board shop,
> for
> > what reason I am trying to comprehend.  Basically, one solder joint
> defect
> > on a board equates to the whole board counting as a defect.  The
> > opportunities are irrelevant - every board gets one opportunity.  When
> the
> > "PPM" numbers are published, which is what they call them, they are
> > outrageously high.  My questions are:
> > Does anyone use Defects per Unit at the board level?
> > If so, what kind of numbers are you seeing.?
> >
> > I am pursuing a change to use real DPMO metrics, but so far I've been
> > unsuccessful.  I even presented IPC-7912, but it was ignored.  Thanks
> in
> > advance for the help.
> >
> > Howard Watson
> > SMT Manufacturing Engineer
> > AMETEK/Dixson
> > ---------------------------------------------------
> > Technet Mail List provided as a free service by IPC using LISTSERV
> 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following text
> in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> > Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> > for additional information, or contact Keach Sasamori at
> [log in to unmask] or
> > 847-509-9700 ext.5315
> > -----------------------------------------------------
> > Grand Junction, CO
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2